Twinned dendrites in Al-Zn alloy with high Zn content (40% wt.%) were successfully prepared by directional solidification. At different directional solidification rates (1000 and 1500 μm/s), microstructures and growth orientation variations of Al twinned dendrite and non-twinned dendrite were characterized. By using the inverted trapezoidal graphite sleeve at 1000 μm/s, Al twinned dendrite were formed to developed feather crystal structures in longitudinal section. Its primary and secondary twinned dendrite were grew along [110] direction. Moreover the deviation angle between [110] direction of Al twinned dendrite and the heat flow direction was about 27.15°. While not using the inverted trapezoidal graphite sleeve at 1000 and 1500 μm/s, Al dendrite was the non-twinned dendrite and the twinned dendrite was not appeared. The experimental results showed that the higher temperature gradient, a certain pulling rate and convection environment were the formation conditions of twinned dendrites.

Go to article

Authors and Affiliations

K. Gao
W. Song
L. Fan
Y. Ding
X. Guo
R. Zhang
Download PDF Download RIS Download Bibtex

Abstract

This study investigated the effect of adding Al–5Ti–1B grain refiner on the solidification microstructure and hot deformation behavior of direct-chill (DC) cast Al–Zn–Mg–Cu alloys. The grain refiner significantly decreased the grain size and modified the morphology. Fine-grained (FG) alloys with grain refiners exhibit coarse secondary phases with a reduced number density compared to coarse-grained (CG) alloys without grain refiners. Dynamic recrystallization (DRX) was enhanced at higher compression temperatures and lower strain rates in the CG and FG alloys. Both particle stimulated nucleation (PSN) and continuous dynamic recrystallization (CDRX) are enhanced in the FG alloys, resulting in decreased peak stress values (indicating DRX onset) at 450°C. The peak stress of the FG alloys was higher at 300-400°C than that of the CG alloys because of grain refinement hardening over softening by enhanced DRX.
Go to article

Authors and Affiliations

Junho Lee
1
ORCID: ORCID
Namhyuk Seo
1
ORCID: ORCID
Sang-Hwa Lee
2
ORCID: ORCID
Kwangjun Euh
2
ORCID: ORCID
Singon Kang
3
ORCID: ORCID
Seung Bae Son
1 4
ORCID: ORCID
Seok-Jae Lee
1 4
ORCID: ORCID
Jae-Gil Jung
1 4
ORCID: ORCID

  1. Jeonbuk National University, Division of Advanced Materials Engineering, Jeonju 54896, Republic of Korea
  2. Korea Institute of Materials Science, Advanced Metals Division, Changwon 51508, Republic of Korea
  3. Dong-A University, Department of Materials Science And Engineering, Busan 49315, Republic of Korea
  4. Jeonbuk National University, Research Center for Advanced Materials Development, Jeonju 54896, Republic of Korea

This page uses 'cookies'. Learn more