Abstract

AISI 316L/TiB2/2p composites were manufactured by HP-HT using different pressures (5 and 7 GPa) and temperatures (900-1300°C), with constant reinforcing particle content 2 vol%. The mechanical properties of the composites were evaluated on the basis of hardness (HV0.3) and compression tests (20°C, 10−5 s−1). The results showed that the role of sintering pressure increased with increasing process temperature. At temperatures of 900°C and pressures of 5 and 7 GPa the difference in measured values of compressive strength was 1-2%, while at 1300°C they reached 20%. At constant pressure of 5 GPa, a change in hardness and compressive strength of 40% were obtained with a temperature change of 900 to 1300°C. Changes in mechanical properties in the composite occurred without substantial changes in density, microstructure, reinforcement phase distribution, and phase composition in the matrix.

Go to article

Authors and Affiliations

P. Kurtyka
Iwona Sulima
ORCID: ORCID
P. Hyjek
L. Jaworska

This page uses 'cookies'. Learn more