Abstract

Paper presents the results of ATD and DSC analysis of two superalloys used in casting of aircraft engine parts. The main aim of the

research was to obtain the solidification parameters, especially Tsol and Tliq, knowledge of which is important for proper selection of

casting and heat treatment parameters. Assessment of the metallurgical quality (presence of impurities) of the feed ingots is also a very

important step in production of castings. It was found that some of the feed ingots delivered by the superalloy producers are contaminated

by oxides located in shrinkage defects. The ATD analysis allows for quite precise interpretation of first stages of solidification at which

solid phases with low values of latent heat of solidification are formed from the liquid. Using DSC analysis it is possible to measure

precisely the heat values accompanying the phase changes during cooling and heating which, with knowledge of phase composition,

permits to calculate the enthalpy of formation of specific phases like γ or γ′.

Go to article

Authors and Affiliations

P. Gradoń
F. Binczyk
J. Cwajna